Skip to content
Welcome to ATM-Casting
Application Notes

Casting industry insights, process notes and production updates from ATM-Casting.

Casting Marking and Traceability: What to Put on a Part Drawing

Published:2026-10-14    Category:Application Notes    Views:3
Marking is normally added to a drawing at the end of the design process, as a note in the corner. That is the wrong place for it. If a part number is unreadable because the characters are cast too small, if a heat number has to be stamped into a fatigue-critical surface, or if a serial number cannot be applied because no accessible surface exists, the problem was created at the design stage and cannot be fixed in the foundry.

Traceability is also the part of the drawing that quality and certification depend on. Without it, a material certificate cannot be tied to a delivered part, and a recall or a non-conformance investigation has nowhere to start.

Why Traceability Matters More Than It Appears

  • Material verification. A certificate for a heat of material is only useful if the part can be linked back to that heat.
  • Non-conformance containment. Investigating a defect requires knowing which production lot, which heat and which process conditions produced the affected parts.
  • Field failure investigation. If a component fails in service, the first question is which batch it came from and what material it was made from.
  • Regulatory and customer requirements. Automotive, aerospace, medical and pressure-equipment standards require defined traceability.
  • Certification. Inspection documents such as EN 10204 Type 3.1 or 3.2 are only meaningful when tied to identifiable parts or lots.

Three Layers of Traceability

Layer What it identifies Where it lives
Part identification Which part this is, and which revision Cast into, stamped on or engraved on the part
Lot and material identification Which heat and which production batch On the part, on the packaging, or on the accompanying documentation
Documentation Proof that the part was made to specification Certificates, test reports and inspection records

The three layers should be consistent with each other. A part marked with a heat number has no traceability value if the certificate does not carry the same heat number, or if two heats are mixed in one delivery without separation.

What to Mark

Data Typical requirement Applies to
Part number Always Every part
Revision or issue letter Where revision affects form, fit or function Most parts
Material grade or designation Common on valves, pumps and pressure parts Castings where mix-up is a risk
Heat number or lot code Required where material certification applies Pressure, automotive, aerospace, medical
Serial number Individual part traceability Safety-critical and single-unit parts
Date or date code Production or shelf-life tracking Where age affects service life
Manufacturer or foundry code Source identification Where multiple sources are approved
Casting process symbol Process identification, sometimes a standard symbol Where the process route must be provable
Directional or safety marks Flow direction, orientation, warning Where incorrect installation is possible

Marking Methods

Method Strength Limitation
Cast-in raised characters Permanent, no extra operation, cannot be removed without destroying the part Fixed at tooling stage; character size limited by casting resolution
Cast-in recessed characters Protected from handling damage Can fill with coating or be hard to read after finishing
Laser marking Small characters, data-matrix codes, high repeatability Shallow depth; may be removed by later machining or may affect corrosion resistance on some alloys
Dot peen marking Fast, works on rough surfaces, deep and durable Creates indentations; not suitable on thin walls or fatigue-critical surfaces
Vibro-etch Low-stress marking Shallow, can be illegible after coating
Stamping Permanent and deep Introduces stress risers; avoid on pressure-retaining or fatigue-critical regions
Ink or adhesive label No part modification Not permanent; unsuitable for heat or solvent exposure
Wired or tied tag Lot-level traceability without marking the part Lost at installation; identification ends at the packing stage

Cast-in marking is usually the best answer for the part number and grade, because it costs nothing per part and it cannot be removed or transposed. Lot-specific data such as a heat number or serial number cannot be cast in, because it varies within one tooling set, so it must be applied afterwards by laser, peen, etch or label.

Design Rules for Cast-in Marking

  • Character height. Keep characters large enough to cast cleanly; very small characters fill poorly and lose legibility. Where the available space is tight, fewer large characters are better than many small ones.
  • Stroke width. Characters need a minimum stroke width to survive filling. Hairline strokes are a common cause of unreadable markings.
  • Relief height. Raised characters should stand proud of the surface enough to be legible but not so much that they are damaged in handling.
  • Draft on characters. Like any other cast feature, raised or recessed characters need draft to release from the wax die.
  • Location. Place marking on a surface that is not machined, not a sealing face, not a fatigue-critical region and not a wear surface.
  • Accessibility. If the part is small or enclosed, check that the marking will actually be readable when the part is installed.
  • Orientation. Specify orientation so that the marking is read the same way on every part.
  • Coating compatibility. If the part will be plated, powder coated or painted, recessed characters may be filled; raised characters may be partially buried.

Connecting Marking to Certification

Marking is the physical end of a documentation chain. Where the customer requires inspection documentation, the drawing should state both the marking requirement and the document type, so the two are designed together.

Document What it establishes Typical marking implication
Material certificate Chemical and mechanical properties of the heat Heat number must appear on the part or on lot packaging
EN 10204 Type 3.1 Inspection document issued by the manufacturer’s own inspection department Lot or part identification must tie back to the certificate
EN 10204 Type 3.2 Inspection document countersigned by an independent inspector Individual or lot marking is normally mandatory
Special process certificates Heat treatment, NDT, coating or testing performed to specification Process lot number must be traceable to the part
First article inspection report Conformance of the production process, not just one part Part and revision marking must match the report

What to Put on the Drawing

  1. Which data fields are required for marking, and which of them are cast-in versus applied.
  2. The exact location of each marking, dimensioned from a datum.
  3. Character height, stroke width and relief height for cast-in marking, with a note on legibility criteria.
  4. Orientation of the marking relative to the part datum frame.
  5. The marking method where it matters, particularly where stamping is prohibited.
  6. Surfaces where marking is not permitted.
  7. The document type to be supplied, and the marking to which it must be traceable.
  8. The handling of multiple heats in one order, including whether each part or only each lot is marked.

Common Mistakes

  • Specifying a marking requirement without specifying the method, leaving the foundry to choose between cast-in and stamping.
  • Designing characters so small that they cannot be cast legibly.
  • Putting cast-in identification on a surface that will later be machined away.
  • Stamping a heat number into a pressure-retaining or fatigue-critical region.
  • Requiring Type 3.2 documentation while allowing bulk-packed, unmarked parts.
  • Allowing multiple heats in a shipment with no way to tell them apart.
  • Forgetting that powder coating or plating can fill or obscure recessed marking.
  • Using a label or tag as the only identification, so traceability ends as soon as the part is unpacked.

About ATM-Casting

ATM-Casting produces investment castings with cast-in part identification and applied lot marking by laser, dot peen or etch, supported by heat-level and lot-level traceability through the production route. Marking requirements are reviewed at the drawing stage, including character size and relief for cast-in marking, permitted marking locations and the documentation type to be supplied. Inspection documents, material certificates and special process records are issued against identifiable parts or lots so that certification can be tied back to the delivered goods.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top