Skip to content
Welcome to ATM-Casting
FAQ

Casting industry insights, process notes and production updates from ATM-Casting.

What materials can you cast?

Published:2026-09-14    Category:FAQ    Views:11
Almost every engineering metal can be cast, and the practical list runs to several hundred alloys. What limits the choice is not the metal itself but the process: which casting route can withstand the melting temperature, what shape the mould can hold, and how many parts you need. Investment casting handles the widest range — carbon and stainless steels, nickel and cobalt superalloys, titanium and copper alloys — because the ceramic shell is destroyed after each pour. Die casting handles the narrowest range but at the lowest unit cost, because it requires a steel die that only non-ferrous alloys will not destroy.

The Four Casting Routes and Their Material Ranges

The material question is really a process question. Sand casting accepts nearly every alloy because sand moulds are cheap and refractory, but it holds loose tolerances. Investment casting accepts nearly every alloy because the shell is expendable, and it holds tighter tolerances on complex shapes. Die casting accepts only non-ferrous alloys because the die is steel. Metal injection moulding is not casting in the traditional sense, but it covers the small, complex, high-volume steel parts that die casting cannot touch.

That gives a simple rule of thumb: if the part is steel or superalloy, the choice is between investment casting, sand casting and MIM. If the part is aluminium, zinc or magnesium in high volume, die casting is in play. Everything else is decided by geometry, quantity and tolerance.

Ferrous Alloys: Carbon, Alloy and Stainless Steels

Ferrous alloys are the largest family in casting, and the reason investment casting dominates general industrial work. Molten steel sits around 1,400 to 1,540 °C, far above anything a die-casting die survives, so every ferrous part is cast into an expendable mould.

Alloy Group Typical Grades Typical Tensile Strength Key Characteristics Typical Parts
Carbon steel 1045, WCB, WCC About 485 to 620 MPa Low cost, weldable, machinable, moderate strength Valve bodies, machinery housings, brackets, pipe fittings
Low-alloy steel 4140, 42CrMo4, 4340 About 655 to 1,000 MPa after heat treatment Higher strength and fatigue resistance than carbon steel Gears, shafts, connecting hardware, load-bearing housings
Austenitic stainless CF8 (304), CF8M (316), CF3MN About 485 MPa, elongation 30% and above Excellent corrosion resistance, non-magnetic, tough at low temperature Pump and valve components, food and dairy equipment, marine hardware
Duplex stainless CD3MN (2205), CD3MWCuN (2507) About 620 to 800 MPa High strength plus chloride stress-corrosion resistance Offshore valves, desalination pumps, chemical process fittings
Martensitic stainless CA15 (410), CA6NM (13-4) About 620 to 900 MPa Hardness and erosion resistance with moderate corrosion resistance Hydro turbine runners, impellers, cutlery, valve trim
Precipitation hardening stainless CB7Cu-1 (17-4 PH), CB7Cu-2 (15-5 PH) Up to about 1,170 MPa in the H900 condition Strength approaching tool steel with stainless corrosion resistance Aerospace fittings, high-strength valves, actuators, fasteners
Tool and wear-resistant steel D2, H13, Hadfield manganese steel Varies with grade and heat treatment High hardness or work-hardening behaviour under impact Wear plates, crusher jaws, die inserts, cutting components

Nickel and Cobalt Superalloys

Superalloys exist for two problems that ordinary steel cannot solve: sustained high temperature, and extreme corrosion. They are cast almost exclusively by the investment route, because the ceramic shell tolerates both the melting temperature and the reactive alloys involved.

Alloy Typical Tensile Strength Service Limits Where It Is Used
Inconel 718 About 1,240 to 1,380 MPa in the aged condition Maintains structural integrity up to roughly 700 °C Jet engine and gas turbine components, high-temperature fasteners
Inconel 625 About 830 to 930 MPa High temperature plus resistance to seawater and acids Marine hardware, chemical process valves, exhaust components
Hastelloy C-276 About 690 to 790 MPa Extreme resistance to oxidising and reducing chemicals Chemical reactor internals, pollution control equipment, acid handling
Monel 400 About 480 to 550 MPa Seawater and hydrofluoric acid environments Marine pump and valve parts, heat exchanger components
Cobalt alloys (Stellite type) Hardness typically 40 to 50 HRC Wear resistance retained at high temperature Valve seats, pump sleeves, hot wear surfaces

Light Alloys: Aluminium, Magnesium and Titanium

Aluminium is cast in enormous volumes by every route, and it is the only metal family where sand, investment and die casting all compete directly. Magnesium is cast primarily by die casting for weight-critical housings, because its low density and thin-wall capability matter more than its strength. Titanium is castable but difficult: it reacts with oxygen and most mould materials at temperature, so titanium casting requires vacuum melting and inert conditions, which puts it firmly in the investment casting world alongside aerospace and medical work.

“Can you die cast aluminium and magnesium on the same machine?” — Not usually. Hot-chamber machines are used for zinc and magnesium, while aluminium requires a cold-chamber machine, and the alloys need separate melt handling to avoid contamination.

Copper-Based Alloys: Bronze and Brass

Copper alloys are cast by sand and investment routes and, in the case of brass, sometimes by die casting. Bronze is chosen for wear and corrosion resistance rather than strength, and remains the default material for bearings, bushings, worm gears and marine hardware because it tolerates boundary lubrication and sliding contact in a way that steel does not. Manganese bronze and aluminium bronze provide much higher strength with good corrosion resistance, which is why they appear in valve bodies, pump impellers and ship propeller hardware.

“Is there a castable material that resists both wear and seawater?” — Aluminium bronze and certain duplex stainless grades come closest. Aluminium bronze combines high strength, good fatigue behaviour and strong resistance to seawater corrosion, which is why it is the standard choice for marine propellers and seawater pump components.

Zinc Alloys

Zinc alloys are the easiest metals to die cast and the cheapest to machine. Zamak 3 and Zamak 5 melt at around 380 to 390 °C, which is far below aluminium, so die life is long and cycle times are short. The trade-offs are high density relative to aluminium, poorer elevated-temperature performance, and lower strength. Applications concentrate in hardware, locks, automotive trim, electrical enclosures and decorative components where the excellent as-cast surface finish pays for itself.

Full Material Comparison

Material Family Typical Melting Range Density (g/cm³) Casting Routes Chosen When
Carbon and low-alloy steel About 1,425 to 1,540 °C 7.8 Investment casting, sand casting Strength and cost matter more than weight or corrosion
Stainless and heat-resistant steel About 1,350 to 1,450 °C 7.6 to 8.0 Investment casting, sand casting Corrosion resistance is the primary requirement
Nickel and cobalt superalloys About 1,260 to 1,400 °C 8.2 to 8.9 Investment casting, vacuum investment casting High temperature or aggressive chemistry rules out steel
Aluminium alloys About 540 to 660 °C 2.6 to 2.8 Die casting, sand casting, investment casting Weight reduction with moderate strength and good conductivity
Magnesium alloys About 470 to 620 °C 1.8 Die casting, sand casting Minimum weight dominates and service temperature is low
Zinc alloys About 380 to 390 °C 6.6 to 6.7 Die casting Complex thin-wall parts with excellent as-cast finish
Copper alloys About 900 to 1,040 °C 8.4 to 8.9 Sand casting, investment casting, some die casting Wear resistance, seawater service or thermal and electrical conductivity
Titanium alloys About 1,600 to 1,660 °C 4.4 to 4.5 Vacuum investment casting Strength-to-weight ratio and biocompatibility justify the cost

What Cannot Be Cast, and Why

  • Refractory metals in ordinary foundries. Tungsten melts near 3,400 °C and molybdenum near 2,600 °C. They can be melted only under vacuum with specialised equipment, so they are produced by powder metallurgy rather than conventional casting.
  • Steel in a die-casting die. Not a material limitation but a tooling one: molten steel destroys the die, so ferrous parts never go to high-pressure die casting.
  • Many structural ceramics and intermetallics. Casting routes exist for some, but they are laboratory or specialised processes rather than production options.
  • Alloys with very wide freezing ranges in thin walls. These are technically castable but prone to incomplete fill and hot tearing, which usually pushes the design toward a different material rather than a different process.

How to Match a Material to a Process

  1. Start with the service environment. Temperature and chemistry decide the alloy family, and the alloy family decides which processes are even available.
  2. Check whether the part is ferrous. If it is, die casting is eliminated and the comparison becomes investment casting against sand casting, machining or MIM.
  3. Weigh the part against the volume. Non-ferrous parts below a few thousand units usually favour investment or sand casting; above that, die casting justifies its tooling.
  4. Define the tolerance and finish up front. A material that casts accurately may still need machining afterwards, and that changes the effective cost of the alloy you selected.
  5. Consider MIM for small, complex, high-volume steel parts. Where investment casting struggles to hold tolerance on parts weighing only a few grams, metal injection moulding delivers near-net shape at volumes that would otherwise require extensive machining.

Common Misconceptions

  • “Casting means sand casting, so the finish will be rough.” Investment casting replicates the wax pattern closely and produces a finish far better than sand casting, often usable with minimal finishing.
  • “A stronger alloy is always the safer choice.” Higher-strength alloys usually cost more, machine less easily and may be less weldable. The right grade is the one that meets the requirement with margin, not the highest number on the chart.
  • “Aluminium is aluminium.” Die-casting grades such as A380 are not the same as casting grades such as A356, and neither behaves like a wrought grade. Alloy selection within a family matters as much as selecting the family.
  • “Magnesium is too flammable to cast.” Molten magnesium requires specific handling precautions, but it is die cast in large volumes for automotive and consumer electronics housings and is well established as a production material.
  • “Titanium cannot be cast.” It can, and investment casting of Ti-6Al-4V is standard for aerospace and medical parts. It simply requires vacuum melting and inert conditions, which is why it is expensive rather than unavailable.

The short version: nearly every engineering metal is castable, and the real constraint is the process combination of melting temperature, tooling material and production volume. Ferrous and superalloy parts go to investment or sand casting, aluminium spans every route, zinc and magnesium belong to die casting, and copper alloys cover wear and marine duties. Pick the alloy from the service environment first, then confirm that a process capable of holding the tolerance and volume is available for it.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat