Stainless Steel Casting Grades Compared: CF8, CF8M, CF3M and CA15

Short answer: Four stainless steel casting grades cover most industrial demand: CF8 is the cast 304, CF8M adds molybdenum as the cast 316, CF3M is the low-carbon version of CF8M for weldments, and CA15 is the martensitic cast 416 for hardness and wear. Choosing among them is a three-question decision — corrosion environment, welding exposure, and strength requirement — not a preference.

What the CF and CA Prefixes Actually Mean

ASTM A356 — the standard naming system for heat-resistant and corrosion-resistant castings — builds grade names from two letters: the first identifies the alloy family, the second the carbon level. C marks the corrosion-resistant (stainless) family. F indicates austenitic structure with iron as the base element; M signals that molybdenum is added; H indicates high carbon; the numeral roughly tracks the wrought counterpart. A marks the martensitic family. So CF8 is an austenitic chromium-nickel casting, CF8M is its molybdenum-bearing sibling, CF3 is a low-carbon austenitic, and CA15 is a martensitic chromium casting. The letters are not decoration: once you can read them, almost every ASTM stainless casting grade on a drawing explains itself before you open the datasheet.

The Austenitic Three: How CF8, CF8M and CF3M Differ

Austenitic stainless steel casting grades are the workhorses of valve, pump, and fittings service — typically poured by investment casting. CF8 sits at roughly 18–21% chromium and 8–12% nickel with carbon up to 0.08%, the direct cast analogue of 304: good general corrosion resistance, excellent toughness, no response to heat treatment beyond solution annealing. CF8M adds 2–3% molybdenum — the cast 316 — which is the single alloying change that matters most for chloride and pitting resistance; where CF8 struggles in brackish water or chemical splash, CF8M holds. Both deliver around 480–520 MPa ultimate tensile strength with 30–40% elongation in the solution-annealed condition. CF3M then changes one variable: carbon drops to a maximum of 0.03%, and that small number reshapes the weld behavior, as covered below.

Why CA15 Is a Different Material Entirely

CA15 is not an austenitic grade with a different label; it is a different metallurgical world. At 11–13% chromium, low nickel, and 0.15% maximum carbon, it solidifies martensitic — the cast equivalent of 416. That structure makes it magnetic, hardenable by quench and temper, and roughly twice as strong as CF8 after heat treatment (typically 620 MPa UTS minimum, with hardness commonly specified in the 28–34 HRC band), but at real cost: about half the elongation, meaningfully lower corrosion resistance, and poor weldability that demands preheat and post-weld tempering. CA15 earns its place where the service is abrasive or where parts need hardness the austenitics cannot give — valve stems, seats, and pump components in non-seawater service. Specifying CA15 for corrosion resistance is a classic mislabel; it is a strength-and-wear grade that happens to be stainless.

The Low-Carbon Question: When CF3M Beats CF8M

Cast austenitic grades carry more carbon than their wrought counterparts, and carbon has a memory: heated between roughly 450 and 850 °C — exactly the temperature band a weld passes through — chromium carbides precipitate at grain boundaries, leaving adjacent zones chromium-starved and vulnerable to intergranular corrosion. This is sensitization. Weld-overlay, fabrication welding to pipe, or any service that reheats the casting makes it real. CF3M’s 0.03% carbon maximum is the insurance policy: with too little carbon available, carbide precipitation cannot get started, which is why weldment and sour-service specs reach for the L-variants — CF3, CF3M, CF3MC — while fully cast bodies that never see a torch can use CF8M and save the alloy surcharge. The rule of thumb is simple: if the part is welded after casting, the low-carbon grade is the default, not the upgrade.

How to Specify: Environment, Welding, Load

Grade Structure Cast Analogue Defining Trait Typical Service
CF8 Austenitic 304 General corrosion resistance, best value Fresh-water valves, general fittings
CF8M Austenitic 316 Molybdenum: pitting and chloride resistance Marine, chemical, pulp service
CF3M Austenitic 316L Low carbon: weld-deposition resistance Welded assemblies, sour and acidic service
CA15 Martensitic 416 Hardenable, magnetic, wear-capable Valve stems, seats, wear parts

Four Questions Before You Lock the Grade

  1. Will the casting be welded after it ships? If yes, move to the low-carbon variant of whichever austenitic your environment requires — this single question re-rates CF8M to CF3M more often than any corrosion chart.
  2. Is chloride present, and above what temperature? Molybdenum answers pitting, but no austenitic grade here resists stress corrosion cracking in hot chlorides; that question points to duplex or nickel alloys instead.
  3. Is the real driver hardness or corrosion? If wear dominates and the environment is mild, CA15’s strength-per-dollar wins; if corrosion dominates, CA15 is a mislabel waiting to fail.
  4. Does the specification name the standard and condition? “CF8M solution annealed per ASTM A351” is a contract; “cast 316” is a conversation.

Q: Why do cast grades use CF names instead of just specifying 304 or 316?
A: Because cast chemistry and properties are not identical to wrought: higher carbon allowances, dendritic structure, and section-size effects all shift the numbers. The CF names exist so the specification matches the material you are actually pouring, not the bar stock the drawing software defaulted to.

Q: Is CF3 the same as CF8 with less carbon?
A: Exactly — CF3 is the low-carbon twin of CF8 (the cast 304L), and CF3M is the low-carbon twin of CF8M (cast 316L). The CF3MC grade then adds nitrogen to the low-carbon molybdenum chemistry for higher strength in the same family.

To Summary

The four stainless steel casting grades most specifications actually fight over resolve into clean roles: CF8 for economical general corrosion service, CF8M when chlorides and pitting enter the picture, CF3M whenever the casting will be welded, and CA15 when hardness and wear matter more than chemistry. Read the letter prefixes, answer the weld question first, and name the standard and condition on the drawing. Do that, and the grade on your stainless steel casting grades callout stops being a habit and becomes an engineering decision.

About ATM-Casting: ATM-Casting is a foundry specializing in investment casting, die casting, and machining of precision metal components for industrial customers worldwide.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top