Skip to content
Welcome to ATM-Casting
Application Notes

Casting industry insights, process notes and production updates from ATM-Casting.

ISO 8062 CT Grades Explained: How to Specify Casting Tolerances on Your Drawing

Published:2026-10-14    Category:Application Notes    Views:5
Most arguments between a designer and a foundry start with a drawing that does not say what the casting is actually allowed to be. A general note reading “tolerances ±0.1 mm unless otherwise stated” is unachievable on any cast surface, and a fully toleranced casting drawing with every dimension individually controlled is unaffordable. ISO 8062 exists to solve both problems: it gives a compact, internationally recognised way to state how tight a casting needs to be, dimension by dimension, without tolerancing every feature separately.

What ISO 8062 Actually Covers

ISO 8062 is the international standard for dimensional and geometrical tolerances on castings. The part that matters for most drawings is ISO 8062-3, which defines general dimensional tolerances, geometrical tolerances and machining allowance grades for castings produced by any process in any cast alloy. It applies to as-cast dimensions, before any secondary machining.

The standard defines sixteen tolerance grades, CT1 through CT16, where CT1 is the tightest and CT16 the loosest. A grade does not give one absolute tolerance; it gives a tolerance band that widens as the nominal dimension grows, which is why the same grade produces a different number for a 20 mm dimension and a 200 mm dimension.

Three points cause most of the confusion in practice:

  • The CT value is the total tolerance band, not a plus-or-minus figure. A CT6 value of 0.64 mm becomes ±0.32 mm if you want a bilateral callout.
  • Grades apply to as-cast surfaces. A machined surface is governed by the machining tolerance, not by the CT grade.
  • No single process can achieve all sixteen grades. Casting processes cluster into bands, and specifying a grade outside the process band simply means the drawing will be quoted with an exception, or not quoted at all.

The CT Value Table

The values below are total tolerance bands in millimetres. To convert to a bilateral tolerance, divide by two.

Nominal dimension (mm) CT4 CT5 CT6 CT7 CT8 CT9 CT10 CT11 CT12
0 – 10 0.26 0.36 0.52 0.74 1.0 1.5 2.0 2.8 4.0
10 – 16 0.27 0.38 0.54 0.78 1.1 1.6 2.2 3.0 4.4
16 – 25 0.28 0.40 0.56 0.82 1.2 1.7 2.4 3.2 4.8
25 – 40 0.30 0.42 0.60 0.86 1.3 1.8 2.6 3.6 5.2
40 – 63 0.32 0.46 0.64 0.92 1.4 2.0 2.8 4.0 5.6
63 – 100 0.36 0.50 0.70 1.0 1.6 2.2 3.2 4.4 6.0
100 – 160 0.40 0.56 0.78 1.1 1.8 2.5 3.6 5.0 7.0
160 – 250 0.50 0.70 1.0 1.4 2.0 2.8 4.0 5.6 8.0
250 – 400 0.56 0.78 1.1 1.6 2.2 3.2 4.4 6.4 9.0
400 – 630 0.64 0.90 1.2 1.8 2.5 3.6 5.0 7.0 10.0
630 – 1000 0.72 1.0 1.4 2.0 2.8 4.0 5.6 8.0 11.0

A worked example makes the practical effect clear. An 80 mm dimension specified at CT6 has a total band of 0.70 mm, so ±0.35 mm. The same dimension at CT5 becomes 0.50 mm total, or ±0.25 mm. Moving one grade tighter on a single dimension looks modest; applying it across a whole casting is where the cost appears.

Which Grades Each Process Can Hold

Grade band Precision level Typical processes
CT1 – CT3 Ultra-high precision Not achievable by casting; requires machining
CT4 – CT6 High precision Silica sol investment casting, high-pressure die casting
CT7 – CT9 Medium precision Water glass investment casting, shell moulding, permanent mould
CT10 – CT12 Standard precision Machine sand casting, gravity die casting
CT13 – CT16 Low precision Hand-moulded sand casting, very large castings

For investment casting the achievable grade depends mainly on the shell system. A silica sol shell, which is the process used for stainless, alloy steel and high-temperature alloys, typically delivers CT5 to CT7, with CT4 achievable on favourable geometry. A water glass shell is cheaper but lands around CT9 to CT11 and produces a rougher surface.

The corollary matters commercially: if a ferrous part needs tighter than CT8, investment casting with a silica sol shell is effectively the only casting route available. Die casting cannot process ferrous metals, and sand casting cannot reach that band.

CT Grades Versus IT Grades

CT grades and IT grades are frequently confused because both are numbered tolerance systems. They are not interchangeable.

System Applies to Range Typical achievement
CT grades (ISO 8062) As-cast dimensions CT1 to CT16 CT4 to CT9 by process
IT grades (ISO 286) Machined dimensions IT01 to IT18 IT5 to IT9 by machining route

A casting held to CT6 behaves roughly like a machined feature at IT11 or IT12 in absolute terms, though the two standards are not directly convertible. The practical implication is straightforward: if a feature genuinely needs IT7 or tighter, it should be designed with machining stock and specified as a machined dimension, not pushed into a tighter CT grade.

How to Specify It on a Drawing

The standard gives three ways to apply a CT grade, and choosing the right one is where most of the value lies.

  1. General tolerances for the whole part. A general note such as “general casting tolerances to ISO 8062-3, CT6” covers every untoleranced dimension. This is the cheapest option and should be the default.
  2. Tighter grades on specific dimensions. Where a group of features needs more control, apply a tighter grade to those dimensions only, rather than to the casting as a whole.
  3. Individual tolerances on critical features. Where a dimension is functionally critical, tolerance it directly. This is the most expensive option per dimension, so it should be reserved for genuinely critical features.

Two supporting callouts are usually needed alongside the grade:

  • The machining allowance grade, so the foundry knows how much stock the machined surfaces carry. Investment casting is typically specified at grade E.
  • Draft angle requirements, if the drawing needs more than the foundry’s standard practice.

What Widens the Tolerance in Practice

Factor Effect
Large overall size Absolute tolerance grows with the nominal dimension, even at the same grade
Wall thickness dimensions Commonly taken one grade coarser than a comparable outside dimension
Abrupt section changes Differential shrinkage causes distortion and warpage
Very thin walls Older or below minimum wall, the casting may not fill consistently
High-melting alloys Hotter pouring increases shell expansion and shrinkage variation
Heat treatment Quenching and normalising can move dimensions after casting
Gate and riser removal Local distortion if cut aggressively or without support
Datums and accumulation Stacked dimensions accumulate variation that a single dimension does not

A Sensible Specification Sequence

  1. Establish which dimensions are functionally critical and which are not. Most cast dimensions are not.
  2. Set a general tolerance grade for the casting, chosen to match what the process can hold: CT6 for silica sol investment casting, unless there is a reason to go tighter.
  3. Apply a tighter grade only to the specific dimensions that need it.
  4. Convert any feature needing IT7 or better into a machined dimension with machining stock, rather than demanding an unrealistic CT grade.
  5. Call out the machining allowance grade for surfaces that will be cut.
  6. State the draft angle requirement if it differs from standard practice.
  7. Ask the foundry for a tolerance feasibility review before releasing the drawing. A grade that cannot be held is worse than no grade at all, because it produces conforming-looking castings and rejected assemblies.

Common Mistakes

  • Applying a blanket plus-or-minus tolerance that ignores the size-dependent nature of casting tolerance.
  • Specifying CT4 or CT5 as a general tolerance, which multiplies cost for features that do not need it.
  • Confusing the total band with a plus-or-minus value, which halves the allowance the foundry is working to.
  • Tolerancing as-cast features as if they were machined, then discovering the process cannot hold them.
  • Omitting the machining allowance grade, leaving the foundry to guess how much stock to leave.
  • Ignoring the “one grade coarser” convention for wall thickness dimensions.
  • Failing to consider that heat treatment and gate removal happen after casting and can move dimensions.

About ATM-Casting

ATM-Casting produces investment castings in carbon and low-alloy steels, stainless and duplex stainless, nickel and cobalt alloys, aluminum and copper alloys, using silica sol shell systems for tighter tolerance work. Dimensional tolerances are specified and inspected to ISO 8062-3 grades, with CMM inspection and first-article reporting available, together with in-house or managed machining for features that require tolerances beyond casting capability. Drawings are reviewed for tolerance feasibility before tooling is released, so that specified grades match what the process can reproducibly hold.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code

Request Callback

WeChat Scan to Visit

WeChat QR Code

WeChat
Back to Top