Tolerance: What Each Process Holds As-Cast
Casting tolerances are standardised rather than negotiated from scratch. ISO 8062-3 defines dimensional casting tolerance grades from CT1 to CT16, where a lower number means a tighter as-cast tolerance. Assigning a CT grade on the drawing turns an argument about “close enough” into a measurable specification both sides can verify.
Three practical points follow from that table. First, die casting’s tolerance advantage is real but concentrated in the tightest grades, and reaching it depends on part size, wall thickness and alloy — a large, thin-walled aluminium casting does not hold CT2 anywhere on the part. Second, investment casting’s process variant matters as much as the process: silica sol shells hold roughly CT5 to CT7 while water glass shells only reach CT9 to CT11, so a tolerance requirement should be matched to the shell system being quoted. Third, tolerance is a percentage of the dimension rather than a fixed number, which is why large castings appear to have generous tolerances in absolute terms and small ones appear impossibly tight.
Flatness and Geometry: The Differences That Actually Bite
Dimensional tolerance is only part of the picture, and for mating surfaces the geometric tolerances matter more. Die casting generally holds flatness around 0.002 in per inch, while investment casting sits near 0.005 in per inch. That difference becomes visible on sealing faces, mounting flanges and anywhere two castings mate without a gasket accommodating the error.
Minimum wall thickness runs the other way in importance rather than direction: die casting can form walls from roughly 0.5 mm in zinc and up to about 2.5 mm in heavier alloys, while investment casting typically needs about 1.5 mm. A design with 1 mm walls points to die casting on capability alone, regardless of volume.
“So die casting is more accurate — why does anyone use investment casting?” — Because tolerance is not the only requirement. Investment casting casts the alloys die casting cannot, has no draft or die-pull constraint, produces denser parts with fewer porosity issues, and requires far less tooling investment at low volume.
Surface Finish: The Tolerance Nobody Writes Down
Surface texture is specified far less often than dimensional tolerance and causes a comparable share of disputes. It also interacts with cost, because a rougher as-cast surface usually means more finishing or more material left for machining.
A typical drawing solves this by convention rather than by analysis: a note such as “dimensional tolerances per ISO 8062-3 CT6 unless otherwise specified,” combined with surfaces marked for machining and a stated as-cast surface finish limit. That approach works because it defines what is acceptable everywhere and names only the exceptions.
How As-Cast Tolerance Turns into Machining Cost
Tolerance only becomes a cost when it forces a second operation. Three mechanisms do that, and each has a different remedy.
The first is a dimension that cannot be held as-cast in either process. The remedy is a machining allowance added to the casting, which costs a little metal and one operation — typically far less than the cost of chasing a tolerance the process cannot hold.
The second is fixture cost. A casting that varies widely between pieces needs either a compliant fixture or an in-process inspection step, and both add cost per part rather than once at tooling.
The third is stack-up. Several cast features that each sit within tolerance can still combine into an out-of-spec assembly, particularly with thin walls and long dimensions. Design reviews catch this before tooling; inspection catches it after, when it is expensive.
Cost Structure: Where the Money Actually Goes
The yield figure is the one most often missing from a buyer’s cost model. If a foundry must melt and process twice the finished weight, then the effective material, energy and labour cost of every delivered part is roughly double what the part weighs. That is why per-kilogram pricing in investment casting looks high compared with the raw alloy price and why part complexity moves the price so much: a thin-walled, intricate part consumes more shell material, cracks more often and sees more scrap than a simple solid block of the same weight, and the cost per kilogram can double as a result.
Typical Per-Kilogram Pricing
Die casting is priced differently, because the dominant variable is machine time and die amortisation rather than metal and labour. Small zinc die castings commonly land between about $0.50 and $3 each, and aluminium die castings are typically quoted per part rather than per kilogram. Per-kilogram comparisons between the two processes therefore mislead: the same finished weight can be far cheaper or far dearer depending on quantity and geometry.
The Break-Even, Restated for Cost
Because the cost structures are inverted, the only meaningful comparison is total cost at your real quantity. Take tooling plus unit price multiplied by quantity for each route and see which total is lower.
Figures are illustrative and intended to show the shape of the decision rather than to predict your quotation. The cross-over in this example sits near 9,300 parts; move the die cost down to $25,000 and it falls to roughly 4,800, while a higher investment casting unit price pushes it the other way. That is why the tooling quote deserves more attention than the unit price in early negotiations.
“Can we get die casting tolerances without die casting tooling costs?” — Sometimes. Sand casting with machined datums, gravity die casting or metal injection moulding can each close part of the gap for specific geometries, and MIM in particular holds tight tolerance on small steel parts at moderate volume.
What Both Quotes Usually Leave Out
- Secondary machining. Whichever process casts the part, features that must be exact are machined. Ask for the machining assumption to be stated explicitly in both quotes.
- Surface treatment. Coating, passivation or painting adds cost and lead time, and thickness may affect dimensions.
- Inspection. Dimensional reports, material certificates, salt spray testing and first article documentation carry their own cost, particularly in regulated industries.
- Scrap and rework allowances. A quotation with an unrealistically low scrap assumption will be adjusted later through price increases or quality disputes.
- Tooling maintenance and replacement. Dies wear and need refurbishment over a long programme; wax dies have a finite pattern life.
- Freight, duties and inventory carrying cost. For offshore supply these can exceed the manufacturing difference between the two processes.
- Cost of change. A design revision costs far less on a wax die than on a hardened steel die, and that asymmetry belongs in the comparison whenever the design is not yet frozen.
Specifying Tolerance Without Overpaying for It
- Assign a CT grade on the drawing rather than leaving tolerance implied. A general note covering all dimensions, with only the exceptions called out, is both cheaper and clearer than tolerancing every feature.
- Reserve tight tolerance for features that need it. Every dimension specified tighter than the process can hold becomes a machining operation with fixtures, inspection and cost attached.
- Match the process variant to the requirement. Silica sol investment casting holds considerably tighter tolerance than water glass, and the price difference is usually smaller than the cost of machining the difference away.
- Never specify tolerance tighter than the function requires on a cosmetic or non-mating surface. It buys nothing and adds cost on every part.
- Ask both suppliers for total cost at your actual annual and lifetime volume, including tooling, finishing, inspection and freight, rather than comparing unit prices.
Common Misconceptions
- “Die casting always has tighter tolerance.” It holds the tighter as-cast capability, but investment casting at CT5 to CT7 is close enough that the difference rarely survives the first machining operation.
- “Cost per kilogram tells you which process is cheaper.” Investment casting is priced largely on metal and labour, die casting largely on machine time and die amortisation. Per-kilogram comparison between them is not meaningful.
- “Tooling cost only matters at low volume.” It matters most at low volume but never disappears; over a long programme it also includes maintenance and eventual replacement.
- “Tighter tolerance is always achievable for a price.” Beyond a point, the process cannot deliver the tolerance as-cast at all, and the honest answer is a machining operation rather than a tighter casting.
- “The cheapest quotation is the cheapest part.” Quotes differ mainly in what they exclude. Comparing exclusions is usually more informative than comparing totals.
The short version: die casting wins on as-cast tolerance and on unit cost once volume passes the cross-over, which for a typical part sits somewhere between a few thousand and roughly ten thousand pieces depending on tooling cost. Investment casting wins below that point, across the whole alloy range, and wherever geometry or design immaturity makes a hardened die a liability. Compare total cost at your real volume, specify tolerance with a CT grade rather than a wish, and confirm which secondary operations each quotation includes.