Do you provide surface treatment services?

Published:2026-09-14    Category:FAQ    Views:12
Yes. Surface treatment is offered as part of the production flow rather than as a separate operation, because on cast, moulded and sintered parts the finish is usually what determines whether the component survives its service environment. The range covers electroplating and electroless plating, passivation and conversion coatings, anodising, organic coatings, magnet-specific coatings, and the mechanical finishing steps that set surface texture. Some specialised processes are run in-house and others through qualified partners, so the practical answer for a specific part is always a question of base material, specification and volume rather than a yes or no.

What Surface Treatment Is Actually For

Finishing does one or more of four jobs, and being clear about which one applies to your part is the difference between an effective specification and an expensive one.

Corrosion protection is the most common. Wear resistance and friction control come second, particularly on sliding, press-fit or valve components. Appearance and tactile finish matter on consumer-facing parts. Functional surface properties — solderability, electrical conductivity, biocompatibility or release behaviour — form the fourth category and often drive the choice in electronics and medical work.

These goals conflict with each other, which is why there is no single best coating. A high-conductivity finish is a poor corrosion barrier; a thick cosmetic coating changes tolerances; a hard wear coating may not survive bending. The specification should name the requirement, not the process.

“Does plating change the dimensions of my part?” — Yes, by roughly twice the coating thickness on any dimension measured across coated surfaces. Always state whether drawing dimensions apply before or after coating, and specify whether threads, bores and sealing faces must be masked.

Coatings for Ferrous Parts

Treatment Typical Thickness Neutral Salt Spray Primary Purpose
Zinc plating 5 to 15 μm About 48 to 96 hours General corrosion protection at low cost
Zinc-nickel alloy 5 to 12 μm 500 hours and above Automotive and high-corrosion environments
Electroplated nickel 5 to 25 μm Moderate; improves substantially over a copper underlayer Appearance, wear and barrier protection
Electroless nickel 5 to 25 μm About 100 to 500 hours depending on thickness and phosphorus content Uniform coverage on complex geometry, corrosion plus wear
Hard chrome 20 to 100 μm and above Good, though chosen primarily for wear Wear resistance on sliding and hydraulic surfaces
Decorative chrome About 0.25 to 0.8 μm over a nickel layer Governed by the nickel underlayer Bright cosmetic appearance
Black oxide Under 2 μm About 0 to 8 hours Indoor appearance with minimal dimensional change
Phosphate coating 2 to 10 μm About 0 to 8 hours alone; far better when oiled or painted Paint base coat and anti-galling in press fits
Tin plating 3 to 10 μm Low Solderability and electrical contact

Zinc-nickel and electroless nickel are the two finishes that most often replace a basic zinc deposit when a specification calls for extended salt spray performance. Hard chrome remains the standard answer for wear, and phosphate is normally specified as a base for paint rather than as a standalone corrosion barrier.

“Will plating cause hydrogen embrittlement in my parts?” — It can. High-strength steels, generally those above about 1,000 MPa tensile strength or 32 HRC, are at risk from acid pickling and electroplating. These parts require a post-plating bake, commonly specified around 190 to 220 °C for several hours, and the requirement must appear on the drawing rather than being assumed.

Treatments for Stainless Steel and Aluminium

Treatment Base Material Typical Thickness Purpose
Passivation Stainless steel No added thickness Removes free iron and restores the passive oxide layer, commonly to ASTM A967
Electropolishing Stainless steel Removes material rather than adding it Combined Ra improvement and passivation for medical and pharmaceutical parts
Anodising, Type II Aluminium 5 to 25 μm Corrosion protection with colour options
Hard anodising, Type III Aluminium 25 to 150 μm Wear resistance plus corrosion protection
Chromate conversion Aluminium, magnesium Under 1 μm Corrosion protection while retaining electrical conductivity; also a paint base
Powder coating Most metals 60 to 120 μm Exterior durability with colour and texture
Electrophoretic coating Most metals 15 to 30 μm Uniform coverage on complex shapes, including internal surfaces

Stainless steel is often assumed to need nothing, which is not quite true after casting or machining. Free iron embedded on the surface from tooling and handling becomes the starting point for corrosion, and passivation removes it. For cast stainless components in marine or chemical service, passivation is normally specified as standard rather than optional.

Coatings for Sintered NdFeB Magnets

Sintered neodymium magnets are porous and corrode readily, so coating is not cosmetic — an uncoated part has no practical service life in a humid environment. The coating must also survive the same temperature as the magnet, which usually means the corrosion requirement and the temperature requirement are specified together.

Coating Typical Thickness Neutral Salt Spray Best Suited To
Zinc 8 to 15 μm About 24 to 48 hours Cost-sensitive indoor and enclosed assemblies
Nickel-copper-nickel 10 to 20 μm About 48 to 72 hours General industrial, motors and sensors
NiCuNi with chemical nickel 4 to 15 μm 48 hours and above Automotive, medical and higher-corrosion environments
Epoxy and polymer systems 15 to 30 μm Extended, typically several hundred hours Outdoor exposure and chemical contact
Parylene 5 to 50 μm Very high, with uniform pinhole-free coverage Thin parts, tight tolerances and medical devices

Coating thickness matters twice on magnets. It adds to the outside dimensions, so tight assemblies need the plated thickness stated on the drawing. It also increases the effective air gap, which slightly reduces the flux a given magnet delivers, so a specification that calls for a very thick coating without considering magnetic performance is usually over-specified.

Mechanical Finishing and Surface Texture

Operation Typical Achievable Ra Effect on the Part
As-cast About 1.6 to 6.3 μm No dimensional change; adequate for non-cosmetic faces
Shot or bead blasting About 1.6 to 3.2 μm Uniform matte texture; commonly used as coating preparation
Vibratory finishing and tumbling About 1.6 to 3.2 μm Mass deburring with edge radius typically 0.05 to 0.2 mm
Machined surfaces About 3.2 to 6.3 μm as standard Functional faces; finer values available with additional passes
Polishing About 0.4 to 0.8 μm Cosmetic improvement and easier cleaning
Mirror polishing Down to about 0.05 μm Reflective surfaces; typically hand-intensive and costly

Texture is worth specifying as a number rather than a description. Terms such as “smooth” or “polished” mean different things to different suppliers, while an Ra value in micrometres is unambiguous. Where a seal, gasket or O-ring contacts the surface, an Ra requirement is often functionally necessary rather than cosmetic.

How to Specify Surface Treatment Correctly

  1. State whether drawing dimensions apply before or after coating. This single sentence prevents most fit and tolerance disputes.
  2. Name the governing standard where one exists. Passivation to ASTM A967, salt spray testing to ASTM B117, or a plating standard such as ASTM B633 gives the supplier a verifiable target.
  3. Give a thickness range rather than a single value. Coating thickness varies across a part, and a range is honest about that variation.
  4. Specify masking requirements. Threads, bores, sealing faces, bearing seats and electrical contact areas often must be left uncoated or given a controlled deposit.
  5. Add the hydrogen embrittlement requirement for high-strength steels, including the bake temperature and duration, rather than leaving it to the plating shop.
  6. Define what the coating must survive, not only what it is. A salt spray duration, an abrasion test or a temperature cycle tells the supplier what the finish has to achieve.

Choosing a Treatment by Requirement

Requirement Recommended Treatment
Corrosion in road-salt or marine exposure Zinc-nickel plating, or NiCuNi with chemical nickel on magnets
Wear on sliding or hydraulic surfaces Hard chrome, electroless nickel or hard anodising on aluminium
Decorative appearance on consumer parts Polishing followed by decorative chrome, powder coating or anodising
Solderability or low electrical resistance Tin, silver or gold plating; chromate conversion on aluminium to retain conductivity
Medical or pharmaceutical cleanliness Electropolishing combined with passivation
Anti-galling in press fits Phosphate coating
Deburring at volume Vibratory finishing or tumbling, accepting a small edge radius

Common Misconceptions

  • “Any coating will do as long as it looks right.” Appearance and corrosion performance are unrelated. A bright cosmetic finish can offer almost no barrier protection.
  • “Stainless steel does not need treatment.” After casting or machining it usually does, because embedded free iron becomes the initiation point for pitting. Passivation removes it.
  • “Thicker coating always lasts longer.” Beyond a point, thick deposits become brittle, flake and crack, and they change part dimensions. Thickness should be specified to a tested requirement.
  • “Salt spray hours describe real service life.” Closed-chamber testing is accelerated and comparative. It ranks finishes reliably but does not predict years of field exposure.
  • “Coatings and tight tolerances coexist without compromise.” A press fit, a thread or a bearing bore usually needs masking or a machined allowance after coating, and that has to be designed in rather than discovered at assembly.

The short version: surface treatment is available across plating, passivation, anodising, organic coatings, magnet coatings and mechanical finishing, and the right choice follows from the requirement rather than the process name. Specify corrosion performance, wear resistance, appearance or function; state thickness and whether dimensions apply before or after coating; add masking and, for high-strength steels, the embrittlement bake requirement. Those four details prevent the great majority of finishing problems.

Chat

Chat Pre-sales Agent

Chat After-sales Agent

Chat

Request Callback

24h Callback Service

Enter your phone number and area code